13μm Mill Finish Aluminum Foil is a standard current collector substrate, and be widely applied in lithium-ion batteries adopting LFP, NCM and NCA cathodes. The base foil supports subsequent advanced surface modification to lower surface resistance, improve conductivity, reinforce active material adhesion, optimize fast-charging and rate performance, and mitigate electrolyte corrosion for longer electrode lifespan.
|
Applicable battery |
Lithium ion battery / Sodium ion battery |
|
Alloy |
AA1100, AA1060, AA1235D |
|
Temper |
H18 |
|
Aluminum Foil Thickness |
8-15µm |
|
Coating Thickness |
3µm (single side/double sides) |
|
Aluminum Foil Width |
300-1550mm |
|
Coating System |
Aqueous slurry |
|
Surface tension |
≥56 dyn/cm |
|
Total Surface density |
38.4±1.5 g/㎡ |
|
Coating surface density |
3.0±0.5 g/㎡ |
|
NMP resistance |
Baked at 130 °C for 10 min. Wiping 200 times with NMP, coating remains intact without peeling |
Product Image

Key Bnenefit of 13μm Mill Finish Aluminum Foil
a. Reduce surface resistance for higher conductivity
b. Enhance bonding strength of active materials to current collectors
c. Improve cell C-rate performance and fast charging capability
d. Prevent electrolyte corrosion and prolong electrode lifespan
e. Mainly applicable to LFP, NCM and NCA systems
leave a message
Scan to wechat :
Scan to Whatsapp :
home
products
Contact Us